AQL, Tray Checks and What a QC Report Should Say

In January, a US fashion jewelry wholesalers and gift shops ordered 240 care and Maintenance and asked for the same cast or stamped as a competitor's sample. What arrived matched the photo and missed the drawing, and 13 pieces had to be reworked at the buyer's expense.

The defect did not surprise us. tarnish in transit is the predictable output of a run where nobody wrote the tolerance down, and it is the first measurement we take on an incoming care and Maintenance. It is written into the care and Maintenance spec sheet that travels with the quote, so the bench and the buyer read the same number.

Care & Maintenance wholesale product photo from the HOLYCOME line in Wuzhou

We did not discount the quote. We changed the gauge, the seat cut, the plating log and the tray rule, and the second run shipped with zero rejects on silver assay at 92.5% minimum and plating adhesion after a 24-hour humidity test. It is written into the care and Maintenance spec sheet that travels with the quote, so the bench and the buyer read the same number.

What North American buyers Check Before They Sign

Price is the first thing compared and the last thing that matters. These four measurements decide the return rate on care and Maintenance, and three of them cost nothing to specify. It is written into the care and Maintenance spec sheet that travels with the quote, so the bench and the buyer read the same number.

Spec pointCommon trade outputHOLYCOME standardCost if missed
Tarnish In Transit on care and MaintenanceInspected visually at the trayGauntlet check on every piece, limit written in the specReturns inside 60 days of wear
Rhodium Adhesion on care and MaintenanceBatch dependent, not loggedThickness and tension logged per lotComplaint after the second season
Weight Shortfall on care and MaintenanceEstimated from nominalGauged per size with go/no-go toolsResize queue and reship cost
Tolerance stack-up on care and MaintenanceQuote states nominal onlyWorst-case band published per SKUFreight and duty drift

None of these are premium features. They cost seconds per piece and they remove the reason a buyer has to inspect twice. It is written into the care and Maintenance spec sheet that travels with the quote, so the bench and the buyer read the same number.

Where USD 8-42 Per Piece Actually Goes

The cost of a care and Maintenance in the USD 8-42 band splits roughly as below. The line buyers challenge most is labor, and it is the line that decides whether the piece survives a season. It is written into the care and Maintenance spec sheet that travels with the quote, so the bench and the buyer read the same number.

Care & Maintenance close-up of setting and finish, HOLYCOME factory sample
Cost lineShareWhat moves it
Base metal or alloy for care and Maintenance34%Alloy choice and casting yield
Stone or melee for care and Maintenance25%Sieve range and lot batching
Setting and finishing labor for care and Maintenance22%Jig design and bench minutes
Plating, polish and QC for care and Maintenance15%Per-tray versus per-piece checks
Packaging and freight for care and Maintenance4%Box grade and DDP versus FOB

If a supplier will not break out the five lines above, the number you are comparing is not a price. It is a total that somebody else assembled from assumptions. It is written into the care and Maintenance spec sheet that travels with the quote, so the bench and the buyer read the same number.

The Three Failures We See Most in Incoming Samples

tarnish in transit

Silver that ships without an anti-tarnish strip browns in a humid container. The strip costs 3 cents and removes the most common arrival complaint.

Our countermeasure is a gauge and a written limit. It adds about 11 seconds per piece and removes the defect from the run rather than from the carton.

rhodium adhesion

A silver surface plated without a palladium strike layer blisters in wear. The strike layer is invisible and essential.

In a 240-piece run this typically shows on 17 of pieces. Catching it means measuring silver assay at 92.5% minimum at the tray level, not inspecting the finished carton.

weight shortfall

A 2.1 g ring shipped at 1.85 g passes a casual check and fails a scale. Publish the weighed average per SKU.

The commercial effect is tarnish claims and replacements, typically USD 4-7 per piece. Buyers who have seen it once put it in the purchase order; buyers who have not usually discover it on the first return.

AQL, Tray Checks and What a QC Report Should Say

This is the question that separates a trading company from a factory, and on care and Maintenance the answer is usually shorter than buyers expect.

There is a version of this that looks cheaper on paper and costs more in practice: quoting the best case on sterling silver pieces and letting the buyer discover the spread. It works once. The second order goes to whichever supplier quoted honestly.

We would rather lose a first order of sterling silver pieces on price than explain a defect after it lands. That position is unusual in this category and it is the reason our reorder share is high.

How a Repeat Order Gets Built

Our process is deliberately boring, because boring is what survives a bulk run with several sets of hands on it. It is written into the care and Maintenance spec sheet that travels with the quote, so the bench and the buyer read the same number.

  1. Spec sheet signed before casting: cast or stamped, tolerances, plating thickness and packing format.
  2. Sample in 3-5 working days from stock components, or about 20 days if a new model is required.
  3. Production photos at three checkpoints: raw cast, post-polish, post-set, with buyer approval at each.
  4. Bulk in 15-20 days under 500 pieces; custom tooling runs 25-30 days.
  5. Pre-shipment QC report with per-tray counts and a retained reference tray for disputes.

A first order at 50 pieces per design is a measurement rather than a purchase. It tells you what silver assay at 92.5% minimum and plating adhesion after a 24-hour humidity test looks like from this line. It is written into the care and Maintenance spec sheet that travels with the quote, so the bench and the buyer read the same number.

The Reject Tray Policy That Decides a Partnership

It is not a marketing point on care and Maintenance. It is the number that decides whether the second order happens.

We run this check per tray rather than per carton because the defect that matters on sterling silver pieces is the one that repeats. A single odd piece is noise; a pattern across one tray is a process problem and it will be in every tray made after it.

The report the buyer receives states the count per tray, the measured average and the outlier count for care and Maintenance. It is deliberately unglamorous, and it is the document that settles most disputes before they start.

MOQ, Mixed Designs and the Real First Order

Every year we see the same omission in care and Maintenance spec sheets, and every year it costs a buyer a season.

The buyers who get the most out of sterling silver pieces treat the first order as a measurement, not as a purchase. They buy a small run, measure the four numbers that matter, and then commit.

We support it directly on care and Maintenance: a 50-piece test run per design, the same gauge standard as a bulk order, and the same retained tray. Small does not have to mean loose.

What the Quote Actually Covers

On care and Maintenance, the difference between a 40-day order and a 90-day order is usually two signatures, not a factory delay.

In US wholesale terms, this is the difference between a landed cost the buyer can plan against and a number that moves after the container ships. For sterling silver pieces, we publish the figure per SKU and hold it for the order window rather than for the calendar year.

Practically, it shows up in three places for sterling silver pieces: the proforma, the QC sheet and the credit note if something goes wrong. All three should quote the same number. When they do not, the argument is about paperwork, not about the product.

What This Means for a First Order

A test run at 50 pieces tells you three things: whether tarnish in transit is controlled, whether packing survives freight, and whether the count is honest. It is written into the care and Maintenance spec sheet that travels with the quote, so the bench and the buyer read the same number.

Buyers who run that measurement before committing a season usually keep the supplier. Buyers who skip it usually pay twice for the same lesson. It is written into the care and Maintenance spec sheet that travels with the quote, so the bench and the buyer read the same number.

Freight, Duty and the Arrival Check

We ship from Guangzhou or Shenzhen, and the port choice follows the carrier rate rather than a fixed habit. It is written into the care and Maintenance spec sheet that travels with the quote, so the bench and the buyer read the same number.

DDP is available for US accounts that want duty and clearance on our side, and it removes the invoice that arrives after the carton clears. It is written into the care and Maintenance spec sheet that travels with the quote, so the bench and the buyer read the same number.

On arrival, weigh a tray and measure ten pieces. Anything outside the band is a claim with evidence rather than a difference of opinion. It is written into the care and Maintenance spec sheet that travels with the quote, so the bench and the buyer read the same number.

Frequently Asked Questions

What is the minimum order for care and Maintenance?

50 pieces per care and Maintenance. Designs mix inside one shipment, so a first order of three designs at 50 pieces each is normal for a new US account. Below 50 we cannot keep the gauge check independent of the shift, which is the part buyers actually pay for on care and Maintenance.

How long does a reorder of the same care and Maintenance take?

12-15 days for care and Maintenance, because the model, the gauge set and the signed spec stay in our system. A first run is longer: 3-5 days for a stock-component sample, about 20 days if a new model is needed, then 15-20 days for bulk under 500 pieces.

Do you supply certificates for care and Maintenance?

assay report per lot for care and Maintenance. Below that threshold we supply a batch report plus per-piece measurement of silver assay at 92.5% minimum, which is what most resellers need at the counter.

What finish do you use on care and Maintenance, and how thick is it?

Rhodium at 0.20 micron minimum on white care and Maintenance, with a palladium strike layer so wear-through reads white rather than yellow. Thickness is logged per lot and appears on the QC sheet, not only in the brochure.

How do you handle a rejected tray of care and Maintenance?

We replace or credit inside the same order cycle. The retained reference tray decides: if tarnish in transit shows on our retained care and Maintenance we own it, and if it appeared in transit we split the assay cost and file with the carrier. A typical exposure on care and Maintenance is tarnish claims and replacements, typically USD 4-7 per piece.

Next Step

If you are quoting care and Maintenance against another supplier, send that quote. We will mark the four lines where the numbers diverge and let you decide. It is written into the care and Maintenance spec sheet that travels with the quote, so the bench and the buyer read the same number.

The factory behind care and Maintenance here is Wuzhou HengliLai Jewelry Co., Ltd., operating since 2009 in Wuzhou, Guangxi, at roughly 60,000 pieces a month. Reach the export desk at service@holycome.com or +86 18078079070 on WhatsApp.